This is Part 4 of our 5 Part Mini Series!
Initial video shows normal weld bead which becomes a sunken weld when the central part of the weld dips below the red line
There is noticeable lack of squeeze pressure indicated by the presence of a sunken weld
The shape of sunken wel has both sides of the weld bead with some symmetry - different than undercut defects
There is noticeable vertical (up and down) movement of the tube surface
Hope you are having a fantastic week, and we'll see you next month with our final Part 5!